Materials & metallurgy

316 / 316L Stainless Steel

The standard Ranger core

316 and 316L stainless steel are austenitic grades with molybdenum added for pitting resistance. 316 is the workhorse of isolation gasket cores: it is weldable, formable, widely available in plate to ASTM A240, and its combination of 16–18% chromium, 10–14% nickel and 2–3% molybdenum gives a pitting resistance equivalent number (PREN) of roughly 24 — enough for most industrial service and for moderate chloride exposure.

In a Protek isolation gasket the alloy is used as the core of the Ranger and Ranger FS constructions, where it carries the bolt load and keeps the gasket geometry stable while a separate sealing element does the sealing. The L grade is the low-carbon version, used where welding is involved; as a machined core plate the two behave the same in service. The core sits inside the sealed gasket, so it is not exposed to the process medium in the way a wetted pipe wall is.

The limits of 316 are chlorides and temperature. In warm, stagnant or crevice conditions — a puddle on a flange face, a bolt hole that holds water, warm seawater — 316 can pit and suffers crevice corrosion, and under tensile stress in the presence of chlorides at temperature it is susceptible to chloride stress corrosion cracking. Those are the cases where the specification moves to duplex 2205, super duplex 2507 or Alloy 625. For standard industrial, utility and moderate-hydrocarbon duty, 316 is the economical and reliable answer.

Composition and standards

316 / 316L Stainless Steel composition and standards
UNS numberS31600 (316) · S31603 (316L)
Composition (typical)16–18% Cr · 10–14% Ni · 2–3% Mo · balance Fe
PREN (typical)~24
Product formPlate / sheet to ASTM A240
Minimum yield (typical)~30 ksi
Sour serviceNACE MR0175 / ISO 15156 within the standard's environmental limits
Protek useStandard core in Ranger and Ranger FS
Configurator option316 SS

Typical properties

Typical properties of 316 / 316L stainless
StandardUNS S31600 / S31603
PREN (typical)~24
Minimum yield (typical)~30 ksi
NotesStandard core. NACE MR0175/ISO 15156 applies within the standard's environmental limits.

Typical values for comparison, not specifications. Actual properties vary by manufacturer, thickness, construction and test method.

Galvanic position

In flowing seawater this material sits at -0.15 V to 0.00 V against a saturated calomel reference. The further apart two materials sit on the series, the harder the couple drives — which is the reason an isolated flange exists: it breaks the circuit before the couple can act.

Seawater potential (vs SCE)
-0.15 to 0.00 V

Flowing seawater at ambient temperature — S.C. Dexter, University of Delaware Sea Grant; ASTM G82; Titanium Information Group (duplex values).

Galvanic tool

Which Protek products use it

PROTEK RANGER

The standard 316 SS core, with a mechanically retained PTFE spring-energized seal.

PROTEK RANGER FS

Steel core with serrated PTFE sealing, fire-safe to API 6FB Third Edition.

Steel core isolation gaskets

How a metal core differs from a laminate retainer under bolt load.

Limits and cautions

  • Pitting and crevice corrosion in warm, stagnant or crevice-bound chloride service, including warm seawater.
  • Chloride stress corrosion cracking under tensile stress with chlorides at temperature.
  • Not the grade to specify for produced water, seawater injection or high-chloride process streams — duplex, super duplex or Alloy 625 are the options there.

Chemical compatibility snapshot

Ratings at ambient temperature from the chemical compatibility matrix, which covers 44 media. A snapshot is shown here — open the tool for the full matrix and the service temperature notes.

316 SS

Holds up against

Water, fresh/cooling · Steam (to 300°F) · Crude oil, sweet · Natural gas, dry · Carbon dioxide, dry

Limited or not recommended

Produced water (H2S/CO2/chlorides) · Hydrochloric acid, dilute (<10%) (not recommended) · Hydrochloric acid, concentrated (not recommended) · Hydrofluoric acid (not recommended) · Sodium hypochlorite (bleach) (not recommended)

Full chemical compatibility matrix
FAQ

Frequently asked questions

What is the difference between 316 and 316L?

+

316L is the low-carbon version of 316, used where welding will take place. As a machined core plate in an isolation gasket the two behave the same in service.

What does PREN ~24 mean?

+

The pitting resistance equivalent number is a comparative measure of resistance to pitting corrosion. About 24 is typical for 316; duplex 2205 is about 35, super duplex 2507 at least 40 and Alloy 625 about 51.

Can a 316 core be used in seawater?

+

Warm or stagnant seawater, and crevice conditions such as a flange face that holds water, are where 316 is limited. Super duplex or Alloy 625 are the usual choices for that service.

Is the core exposed to the process medium?

+

The core sits inside the sealed gasket and is not a wetted surface in the way the pipe wall is. The core grade is chosen for the environment the joint sees and for the duty of the assembly.