Materials & metallurgy

Duplex 2205

Higher strength, better chloride resistance

Duplex 2205 is a two-phase austenitic-ferritic stainless steel: about 22% chromium, 5% nickel and 3% molybdenum with nitrogen added, giving a typical PREN of about 35. The duplex microstructure roughly doubles the yield strength compared with 316 — around 65 ksi typical minimum yield — and it resists chloride stress corrosion cracking far better than the austenitic grades.

In an isolation gasket core, that combination is useful for two separate reasons. The higher strength means the core carries a concentrated raised-face seating load with less deflection, and the better chloride resistance extends the range of environments the joint can live in — produced water, brackish and cooling water, and coastal atmospheres where 316 would be marginal. Duplex is one of the core options in the Ranger configurator.

The limitation to know is toughness at low temperature. Duplex steels lose fracture toughness below roughly −50°F, so a duplex core is not the right choice for cold service or for a joint that will see a cryogenic upset. Above that limit, and within the environmental limits of NACE MR0175 / ISO 15156 for sour service, duplex 2205 is a practical step up from 316 without going to a nickel alloy.

Composition and standards

Duplex 2205 composition and standards
UNS numberS31803 / S32205
Composition (typical)~22% Cr · ~5% Ni · ~3% Mo · N · balance Fe
PREN (typical)~35
Minimum yield (typical)~65 ksi — about twice 316
Low-temperature limitToughness falls below about −50°F
Sour serviceNACE MR0175 / ISO 15156 limits apply
Protek useCore option in Ranger and Ranger FS
Configurator optionDuplex

Typical properties

Typical properties of Duplex 2205
StandardUNS S31803 / S32205
PREN (typical)~35
Minimum yield (typical)~65 ksi
NotesRoughly twice the yield of 316 with better chloride resistance. Duplex steels lose toughness below about −50°F.

Typical values for comparison, not specifications. Actual properties vary by manufacturer, thickness, construction and test method.

Galvanic position

In flowing seawater this material sits at -0.07 V against a saturated calomel reference. The further apart two materials sit on the series, the harder the couple drives — which is the reason an isolated flange exists: it breaks the circuit before the couple can act.

Seawater potential (vs SCE)
-0.07 V

Flowing seawater at ambient temperature — S.C. Dexter, University of Delaware Sea Grant; ASTM G82; Titanium Information Group (duplex values).

Galvanic tool

Which Protek products use it

PROTEK RANGER

Selected as the core option for chloride-bearing or higher-load service.

PROTEK RANGER FS

The fire-safe construction with the same core option.

Steel core isolation gaskets

Why a steel core is used above Class 900.

Limits and cautions

  • Fracture toughness drops below roughly −50°F, so it is not a cold-service material.
  • Sour service is limited by NACE MR0175 / ISO 15156 rather than by a general rating.
  • More expensive than 316 — specify it for the chloride or load reason, not by default.

Chemical compatibility snapshot

Ratings at ambient temperature from the chemical compatibility matrix, which covers 44 media. A snapshot is shown here — open the tool for the full matrix and the service temperature notes.

Duplex 2205

Holds up against

Water, fresh/cooling · Steam (to 300°F) · Crude oil, sweet · Crude oil, sour (H2S) · Natural gas, dry

Limited or not recommended

Hydrochloric acid, dilute (<10%) · Hydrochloric acid, concentrated (not recommended) · Hydrofluoric acid (not recommended) · Sodium hypochlorite (bleach) · Chlorine, wet (not recommended)

Full chemical compatibility matrix
FAQ

Frequently asked questions

What makes duplex 2205 different from 316?

+

A two-phase austenitic-ferritic microstructure with nitrogen: roughly twice the yield strength, a PREN of about 35 and much better resistance to chloride stress corrosion cracking.

Can duplex 2205 be used at low temperature?

+

Not below roughly −50°F, where duplex steels lose fracture toughness. Cold service calls for an austenitic grade or a nickel alloy.

Is duplex 2205 suitable for sour service?

+

Within the environmental limits of NACE MR0175 / ISO 15156 — that is an engineering assessment for the specific partial pressure, temperature and chloride level.

How do I specify a duplex core?

+

Choose Duplex as the core material in the isolation kit configurator, or state it on the enquiry with the service conditions.